| Parameter | Value |
|---|---|
| Orderable part number | EREC3006TL |
| Repetitive peak reverse voltage (VRRM) | 600 V |
| Maximum RMS voltage (VRMS) | 420 V |
| Maximum DC blocking voltage (VDC) | 600 V |
| Average forward current (IF(AV)) | 30 A at Tmb ≤ 115 °C |
| Peak forward surge current (IFSM) | 270 A, 8.3 ms half sine |
| Forward voltage (VF) | 2.7 V max (typ 2 V), IF=30 A Tj=25 °C |
| Reverse current at VRRM, 25 °C | 5 uA max |
| Reverse recovery time (trr) | 19 ns typ / 23 ns max |
| Reverse recovery charge (Qrr) | 55 nC typ |
| Peak reverse recovery current (IRM) | 3.8 A typ |
| Thermal resistance, junction to ambient | 44 °C/W |
| Thermal resistance, junction to case | 1 °C/W |
| Operating junction and storage temperature | -55 °C to +150 °C |
| Package | TO-247J-2L |
| Mounting | Through-hole |
| Weight | 5.75 g typical |
| Polarity | Cathode marked on the tab |
| Recovery class | Hyperfast |
| RoHS | Compliant, halogen free |
| Data sheet | Eaton Technical Data ELX1410 |
Rating conditions (ambient or case temperature, test current, dI/dt) are
as printed in Eaton Technical Data ELX1410; the values above are taken from the
table for this part number, not from a family summary.
The reverse leakage is the price of the fast die. It is specified at 25 °C and again at the high temperature, and the second figure is often fifty to a hundred times the first. On a 150 °C design the hot value is the one that matters.
30 A through a 2.7 V drop is 81 W of conduction loss, and that is the figure the thermal path has to carry. The switch in the same loop dissipates on its own, so the diode is rarely the only heat source on the tab.
Against 44 °C/W the same 81 W lifts the junction by about 3564 °C above the reference point of that figure. With 150 °C allowed, that leaves the margin the ambient or the heatsink has to stay inside.
The 600 V repetitive rating comes with a 420 V RMS figure, which is the 0.707 factor of the same sine. On a 230 V mains input the peak is already 325 V before any surge, so the margin here is what the transient clamp has to respect.
The surge rating is 9 times the average current, but only for one 8.3 ms half sine. Inrush that repeats on every power-up accumulates heat and has to be checked against the transient thermal impedance curve instead.
Hyperfast and superfast are relative terms. The die is a P-I-N structure with a thin drift region and lifetime control, so the stored charge that has to be swept out at turn-off is small. That is what makes the recovery time a few tens of nanoseconds instead of a few microseconds.
On a bridge or a PFC stage, keep the return path of each diode pair on the same layer. The recovery currents of the two halves then share a path instead of crossing the board through vias.
Can these be paralleled?
Only with care. Forward voltage has a positive temperature coefficient at rated current, which helps sharing, but the recovery characteristics of two dice are never identical. Use a single larger part where the current allows it.
How is the heatsink sized?
Multiply the conduction loss by the junction-to-case thermal resistance to get the rise to the case, then add the case-to-heatsink and heatsink-to-ambient rises. The junction-to-ambient figure in the table already includes a defined copper area and is only valid for that layout.
What package should a 600 V, 10 A design use?
The choice is thermal, not electrical. A TO-252 carries the current but needs the copper to do it; a TO-220 or TO-247 gives a metal tab and a real thermal path. The same die in the two packages has very different usable current.