Eaton HC7-R47-R Powder Iron Inductor 0.53 uH, Isat 27.5 A
Eaton HC7-R47-R Powder Iron Inductor 0.53 uH, Isat 27.5 A

Eaton HC7-R47-R Powder Iron Inductor 0.53 uH, Isat 27.5 A

Share
Eaton HC7-R47-R: powder iron high-current inductor, 0.53 uH ±20%, 23.4 A Irms, Isat 27.5 A, DCR 1.6 mOhm, 13.8 mm long.
    • Product Details
    • Download

    Eaton HC7-R47-R Powder Iron Inductor 0.53 uH, Isat 27.5 A

    HC7-R47-R at a glance: powder iron high-current inductor, 0.53 uH ±20%, 23.4 A Irms, Isat 27.5 A (15% rolloff), DCR 1.6 mOhm, 13.8 mm long.

    Electrical Specifications

    ParameterValue
    Orderable part numberHC7-R47-R
    OCL (open circuit inductance)0.53 uH ±20%
    Irms (DC, 40 °C rise)23.4 A
    Isat (15% rolloff)27.5 A
    Isat2 (30% rolloff)51.9 A
    DCR typical @ +20 °C1.6 mOhm
    Volt-time rating (V-us)3.83
    Package13.8 mm long
    Height5.5 mm
    MountingSurface mount
    Operating temperature-40 °C to +155 °C (ambient plus self-heating)
    QualificationCommercial grade
    RoHSCompliant, -R suffix
    Data sheetEaton Technical Data 4116

    Dimensions and Pad Layout

    HC7-R47-R mechanical dimensions and pad layout

    Drawing reproduced from Eaton Technical Data 4116: outline with
    rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
    the drawing itself.

    What the Numbers Mean

    Powder iron is the material choice that gives this family its soft saturation curve and its stable inductance over temperature. There is no thermal aging of the binder, so the inductance you measure on day one is the inductance you have after a thousand thermal cycles.

    At the rated 23.4 A the winding dissipates about 0.876 W in copper alone, using the typical DCR of 1.6 mOhm. That figure is the floor of the loss budget: it assumes the current is pure DC, and any ripple adds to it.

    Saturation is quoted as 15% rolloff. At that point the inductance has fallen to the stated fraction of its nominal value – the part is not damaged there, it simply stops behaving like the inductance on the label. Design the peak current to stay inside that boundary with margin for tolerance.

    At Isat the part holds about 200 uJ. On a multiphase rail that is the energy per phase available to bridge a load step, which sets how much bulk capacitance the controller still needs.

    The second saturation column, 51.9 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.

    Where This Series Fits

    The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.

    Within the HC7 family this is value 2 of 7, in a range that runs from 0.22 uH to 4.81 uH.

    Compared with its neighbours in the table, HC7-1R0-R trades 15.5 A of rated current for the next inductance step, which is the usual compromise in this family.

    • Core material: powder iron core, 13.8 mm long body at 5.5 mm.
    • Typical applications: multi-phase regulators; voltage regulator modules (vrms); distributed power systems dc-dc converters; desktop and server vrms and evrds; point-of-load (pol) modules; field programmable gate array (fpga) dc-dc converters.
    • The two saturation columns are different criteria, not two measurements of the same thing. Pick the rolloff you can tolerate in the application and stay with that column.

    Sizing It Into a Design

    Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 1.6 mOhm becomes roughly 2.45 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.

    Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.

    • Check the volt-time rating against the applied V-us at the switching frequency.
    • Confirm the part marking is visible after placement for traceability.
    • Check the volt-time rating against the applied V-us at the switching frequency.

    Frequently Asked Questions

    Does the inductance drift with age?
    The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.

    What is soft saturation?
    The inductance falls gradually as current rises instead of collapsing at a threshold. A powder core with a distributed gap behaves this way, which keeps the converter stable through a load transient.

    Is the part shielded?
    The winding is enclosed by the powder core, so the external field is small. It is not a closed ferrite shield, but the fringing field is low enough for dense board layouts.

    Shenzhen Gaorunxin Technology Co., Ltd

    Online message

    Shenzhen Gaorunxin Technology Co., Ltd

    Related Products