| Parameter | Value |
|---|---|
| Orderable part number | HC8-3R5-R |
| OCL (open circuit inductance) | 3.52 uH ±20% |
| Irms (DC, 40 °C rise) | 8.5 A |
| Isat (15% rolloff) | 8.7 A |
| Isat2 (30% rolloff) | 15.3 A |
| DCR typical @ +20 °C | 16.5 mOhm |
| Volt-time rating (V-us) | 7.5 |
| Package | 10.9 x 10.4 mm |
| Height | 4.0 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data 4120 |

Drawing reproduced from Eaton Technical Data 4120: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
Powder iron is the material choice that gives this family its soft saturation curve and its stable inductance over temperature. There is no thermal aging of the binder, so the inductance you measure on day one is the inductance you have after a thousand thermal cycles.
With 16.5 mOhm typical, the I-squared-R loss at the full 8.5 A rating is about 1.19 W. Compare that against the converter output power before deciding whether the part needs airflow or a copper pour under it.
Saturation is quoted as 15% rolloff. At that point the inductance has fallen to the stated fraction of its nominal value – the part is not damaged there, it simply stops behaving like the inductance on the label. Design the peak current to stay inside that boundary with margin for tolerance.
Stored energy at Isat is about 133 uJ, which is the energy the inductor hands to the load during a transient before the control loop reacts.
The second saturation column, 15.3 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
The HC8 family spans 0.175 uH to 47.3 uH; this row sits at position 7 of 16.
One step down the table, HC8-2R6-R, sits at 2.65 uH with 10.2 A and 11.4 mOhm – the lower inductance buys about 2.2 A of extra current in the same body.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 16.5 mOhm becomes roughly 25.3 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
How do I estimate the inductance at my operating current?
Read it off the inductance-versus-DC-bias curve in the data sheet at the actual bias. The curve, not the OCL value, is what sets the ripple at load.
Is the part shielded?
The winding is enclosed by the powder core, so the external field is small. It is not a closed ferrite shield, but the fringing field is low enough for dense board layouts.
Does the inductance drift with age?
The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.
Shenzhen Gaorunxin Technology Co., Ltd
Shenzhen Gaorunxin Technology Co., Ltd