| Parameter | Value |
|---|---|
| Orderable part number | HC8LP-1R2-R |
| OCL (open circuit inductance) | 1.35 uH ±20% |
| Irms (DC, 40 °C rise) | 12.4 A |
| Isat (15% rolloff) | 10.1 A |
| Isat2 (30% rolloff) | 18.7 A |
| DCR typical @ +20 °C | 7.5 mOhm |
| Volt-time rating (V-us) | 2.6 |
| Package | 10.9 x 10.4 mm |
| Height | 3.5 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data 4126 |

Drawing reproduced from Eaton Technical Data 4126: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
Powder iron is the material choice that gives this family its soft saturation curve and its stable inductance over temperature. There is no thermal aging of the binder, so the inductance you measure on day one is the inductance you have after a thousand thermal cycles.
With 7.5 mOhm typical, the I-squared-R loss at the full 12.4 A rating is about 1.15 W. Compare that against the converter output power before deciding whether the part needs airflow or a copper pour under it.
The saturation rating reads 15% rolloff. Treat it as the edge of the linear region: below it the inductance is within tolerance, above it the value droops. For a current-mode converter that means the peak current at the worst-case load step is what must fit under this number.
Energy storage at the saturation current is around 68.9 uJ, the number that connects the inductance and the current rating into a single transient figure.
The second saturation column, 18.7 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
Of the 16 values listed for HC8LP, this is the 4th, in a family covering 0.17 uH to 47.9 uH.
Compared with its neighbours in the table, HC8LP-1R9-R trades 5.5 A of rated current for the next inductance step, which is the usual compromise in this family.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 7.5 mOhm becomes roughly 11.5 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
Why is the DCR higher than a ferrite part of the same size?
Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.
Is the part shielded?
The winding is enclosed by the powder core, so the external field is small. It is not a closed ferrite shield, but the fringing field is low enough for dense board layouts.
Is the part shielded?
The winding is enclosed by the powder core, so the external field is small. It is not a closed ferrite shield, but the fringing field is low enough for dense board layouts.
Shenzhen Gaorunxin Technology Co., Ltd
Shenzhen Gaorunxin Technology Co., Ltd