Eaton HC9-100-R 10.9 uH SMD Power Inductor, 22 V-us
Eaton HC9-100-R 10.9 uH SMD Power Inductor, 22 V-us

Eaton HC9-100-R 10.9 uH SMD Power Inductor, 22 V-us

Share
Eaton HC9-100-R: powder iron high-current inductor, 10.9 uH ±15%, 8.5 A Irms, Isat 8.6 A, DCR 14 mOhm, 13.1 x 14.1 mm.
    • Product Details
    • Download

    Eaton HC9-100-R 10.9 uH SMD Power Inductor, 22 V-us

    HC9-100-R at a glance: powder iron high-current inductor, 10.9 uH ±15%, 8.5 A Irms, Isat 8.6 A (20% rolloff), DCR 14 mOhm, 13.1 x 14.1 mm.

    Specification Table

    ParameterValue
    Orderable part numberHC9-100-R
    OCL (open circuit inductance)10.9 uH ±15%
    Irms (DC, 40 °C rise)8.5 A
    Isat (20% rolloff)8.6 A
    Isat2 (30% rolloff)12.5 A
    DCR typical @ +20 °C14 mOhm
    Volt-time rating (V-us)22
    Package13.1 x 14.1 mm
    Height7.5 mm
    MountingSurface mount
    Operating temperature-40 °C to +155 °C (ambient plus self-heating)
    QualificationCommercial grade
    RoHSCompliant, -R suffix
    Data sheetEaton Technical Data DS4312

    Mechanical Dimensions & Pad Layout

    HC9-100-R mechanical dimensions and pad layout

    Drawing reproduced from Eaton Technical Data DS4312: outline with
    rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
    the drawing itself.

    The Figures Explained

    A powder core with a non-organic binder is a deliberately conservative choice: it trades a little permeability for predictable behaviour at high current and high temperature. The result is an inductor that stays linear enough for a current-mode loop to be designed around it.

    Copper loss at the rated current works out to roughly 1.01 W from a typical DCR of 14 mOhm at 8.5 A. It is the number to start a thermal stack-up with, before core loss and before AC resistance rise.

    Isat is specified as 20% rolloff, so the number is a rolloff criterion rather than an absolute maximum. The useful working range extends a little beyond it on a soft saturation core, but the loop compensation has to be designed for the inductance that remains.

    The core stores roughly 403 uJ at the saturation point – a useful figure when sizing the output capacitance that has to absorb the same transient.

    The second saturation column, 12.5 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.

    Where This Series Fits

    The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.

    Of the 12 values listed for HC9, this is the 9th, in a family covering 0.218 uH to 49.2 uH.

    One step down the table, HC9-6R8-R, sits at 7.45 uH with 10.3 A and 9.4 mOhm – the lower inductance buys about 4 A of extra current in the same body.

    • Core material: powder iron core, 13.1 x 14.1 mm body at 7.5 mm.
    • Typical applications: multi-phase regulators; voltage regulator modules (vrms); distributed power systems dc-dc converters; desktop and server vrms and evrds; point-of-load (pol) modules; field programmable gate array (fpga) dc-dc converters.
    • The two saturation columns are different criteria, not two measurements of the same thing. Pick the rolloff you can tolerate in the application and stay with that column.

    Sizing and Layout Notes

    Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 14 mOhm becomes roughly 21.4 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.

    Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.

    • Use the inductance-versus-DC-bias curve for the ripple calculation, not OCL.
    • Check that the inductance at the working DC bias still meets the ripple target.
    • Check the volt-time rating against the applied V-us at the switching frequency.

    Frequently Asked Questions

    Why is the DCR higher than a ferrite part of the same size?
    Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.

    Does the inductance drift with age?
    The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.

    Does the inductance drift with age?
    The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.