Eaton HC9-470-R 49.2 uH Powder Iron Inductor, 3.65 A
Eaton HC9-470-R 49.2 uH Powder Iron Inductor, 3.65 A

Eaton HC9-470-R 49.2 uH Powder Iron Inductor, 3.65 A

Share
Eaton HC9-470-R: powder iron high-current inductor, 49.2 uH ±15%, 3.65 A Irms, Isat 3.9 A, DCR 72.3 mOhm, 13.1 x 14.1 mm.
    • Product Details
    • Download

    Eaton HC9-470-R 49.2 uH Powder Iron Inductor, 3.65 A

    HC9-470-R at a glance: powder iron high-current inductor, 49.2 uH ±15%, 3.65 A Irms, Isat 3.9 A (20% rolloff), DCR 72.3 mOhm, 13.1 x 14.1 mm.

    Ratings at a Glance

    ParameterValue
    Orderable part numberHC9-470-R
    OCL (open circuit inductance)49.2 uH ±15%
    Irms (DC, 40 °C rise)3.65 A
    Isat (20% rolloff)3.9 A
    Isat2 (30% rolloff)5.7 A
    DCR typical @ +20 °C72.3 mOhm
    Volt-time rating (V-us)44.8
    Package13.1 x 14.1 mm
    Height7.5 mm
    MountingSurface mount
    Operating temperature-40 °C to +155 °C (ambient plus self-heating)
    QualificationCommercial grade
    RoHSCompliant, -R suffix
    Data sheetEaton Technical Data DS4312

    Dimensions and Pad Layout

    HC9-470-R mechanical dimensions and pad layout

    Drawing reproduced from Eaton Technical Data DS4312: outline with
    rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
    the drawing itself.

    Reading the Data Sheet

    A powder core with a non-organic binder is a deliberately conservative choice: it trades a little permeability for predictable behaviour at high current and high temperature. The result is an inductor that stays linear enough for a current-mode loop to be designed around it.

    At the rated 3.65 A the winding dissipates about 0.963 W in copper alone, using the typical DCR of 72.3 mOhm. That figure is the floor of the loss budget: it assumes the current is pure DC, and any ripple adds to it.

    Saturation is quoted as 20% rolloff. At that point the inductance has fallen to the stated fraction of its nominal value – the part is not damaged there, it simply stops behaving like the inductance on the label. Design the peak current to stay inside that boundary with margin for tolerance.

    Energy storage at the saturation current is around 374 uJ, the number that connects the inductance and the current rating into a single transient figure.

    The second saturation column, 5.7 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.

    Where This Series Fits

    The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.

    Of the 12 values listed for HC9, this is the 12th, in a family covering 0.218 uH to 49.2 uH.

    Compared with its neighbours in the table, HC9-330-R trades 0 A of rated current for the next inductance step, which is the usual compromise in this family.

    • Core material: powder iron core, 13.1 x 14.1 mm body at 7.5 mm.
    • Typical applications: multi-phase regulators; voltage regulator modules (vrms); distributed power systems dc-dc converters; desktop and server vrms and evrds; point-of-load (pol) modules; field programmable gate array (fpga) dc-dc converters.
    • The two saturation columns are different criteria, not two measurements of the same thing. Pick the rolloff you can tolerate in the application and stay with that column.

    Putting It to Work

    Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 72.3 mOhm becomes roughly 111 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.

    Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.

    • Check that the inductance at the working DC bias still meets the ripple target.
    • Check that the inductance at the working DC bias still meets the ripple target.
    • Compare the two saturation columns before fixing the current limit in the controller.

    Frequently Asked Questions

    Why is the DCR higher than a ferrite part of the same size?
    Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.

    How do I estimate the inductance at my operating current?
    Read it off the inductance-versus-DC-bias curve in the data sheet at the actual bias. The curve, not the OCL value, is what sets the ripple at load.

    Why is the DCR higher than a ferrite part of the same size?
    Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.

    Shenzhen Gaorunxin Technology Co., Ltd

    Online message

    Shenzhen Gaorunxin Technology Co., Ltd

    Related Products