| Parameter | Value |
|---|---|
| Orderable part number | HC9-R20-R |
| OCL (open circuit inductance) | 0.218 uH ±15% |
| Irms (DC, 40 °C rise) | 46.7 A |
| Isat (20% rolloff) | 65 A |
| Isat2 (30% rolloff) | 95 A |
| DCR typical @ +20 °C | 0.5 mOhm |
| Volt-time rating (V-us) | 2.87 |
| Package | 13.1 x 14.1 mm |
| Height | 7.5 mm |
| Mounting | Surface mount |
| Operating temperature | -40 °C to +155 °C (ambient plus self-heating) |
| Qualification | Commercial grade |
| RoHS | Compliant, -R suffix |
| Data sheet | Eaton Technical Data DS4312 |

Drawing reproduced from Eaton Technical Data DS4312: outline with
rated mm dimensions, recommended pad layout and winding schematic. Tolerances are stated on
the drawing itself.
Powder iron is the material choice that gives this family its soft saturation curve and its stable inductance over temperature. There is no thermal aging of the binder, so the inductance you measure on day one is the inductance you have after a thousand thermal cycles.
Copper loss at the rated current works out to roughly 1.09 W from a typical DCR of 0.5 mOhm at 46.7 A. It is the number to start a thermal stack-up with, before core loss and before AC resistance rise.
Saturation is quoted as 20% rolloff. At that point the inductance has fallen to the stated fraction of its nominal value – the part is not damaged there, it simply stops behaving like the inductance on the label. Design the peak current to stay inside that boundary with margin for tolerance.
Energy storage at the saturation current is around 460 uJ, the number that connects the inductance and the current rating into a single transient figure.
The second saturation column, 95 A at 30% rolloff, is the same core taken further into rolloff. The ratio between the two columns is a direct measure of how soft the curve is: a part with a wide gap between them loses inductance slowly and tolerates a larger transient peak.
The HC powder family sits at the higher-inductance end of the high-current range: from a fraction of a microhenry up to tens of microhenry, on surface-mount bodies with powder iron cores. Every row carries two saturation columns so the rolloff criterion can be chosen explicitly.
Within the HC9 family this is value 1 of 12, in a range that runs from 0.218 uH to 49.2 uH.
Compared with its neighbours in the table, HC9-R47-R trades 0 A of rated current for the next inductance step, which is the usual compromise in this family.
Copper resistance rises with temperature, so at the +155 °C limit the maximum DCR of 0.5 mOhm becomes roughly 0.765 mOhm. That is the figure to put into a hot-enclosure loss calculation; the +20 °C column is a bench number.
Design note: use the 30% rolloff column only if the loop can tolerate the inductance droop; the tighter column keeps more inductance at the cost of a lower usable peak current.
Does the inductance drift with age?
The binder is non-organic and the core is not gapped with adhesive, so thermal aging of the magnetic path is not a mechanism here. The value is stable across thermal cycles.
How do I estimate the inductance at my operating current?
Read it off the inductance-versus-DC-bias curve in the data sheet at the actual bias. The curve, not the OCL value, is what sets the ripple at load.
Why is the DCR higher than a ferrite part of the same size?
Iron powder has lower permeability, so more turns are needed for the same inductance, and more turns mean more copper. The compensation is the much higher saturation flux density.
Shenzhen Gaorunxin Technology Co., Ltd